EN 10277-2 Standard

W.NR.: 1.0543/E335GC

Non-Alloy Steel For Structural Purposes

Heat analysis according to the EN 10277-2 standard

C % Si % Mn % P % S % N % Cu %
From
To 0,045 0,045 0,012

According to the EN 10277-2 standard

Thickness mm Rolled + Peeled Rolled
( +SH )
Cold Drawn
( +C )
Hardness HB Rm (MPa) Rp0,2  minimum Rm (MPa) A5 %
(MPa) minimum
≥5≤10 540 da 700 a 1050 5
>10≤16 480 da 680 a 970 6
>16≤40 da 169 a 211 da 570 a 710 390 da 640 a 930 7
>40≤63 da 169 a 211 da 570 a 710 340 da 620 a 870 8
>63≤100 da 169 a 211 da 570 a 710 295 da 570 a 810 8

* Delivery condition: as rolled.

Weldability:
Failing any prescriptions concerning chemical composition, no technical data about this steel weldability are available.

Notes:

CORRESPONDENCE WITH OTHER STANDARDS (purely as an indication):

EN 10025-2:04 EN 10025:90 UNI 7070 DIN 17 100 NF A35-501
 E335  Fe 590-2  Fe 590  St 60-2  A 60-2