AISI: 316L ESR
EN: 1,4441
C max: 0,030
Mn max: 2
P max: 0,025
S max: 0,010
Si max: 0,75
Cr: 17÷19
Ni: 13÷14,5
Mo: 2,5÷3
Altri: N=0,1 max – Cu=0,5 max

Chemical Analysis
Characteristics
The basic material is 316L which is subjected to the ESR method (Electro Slag Remelting) a distillation process, which eliminates all kinds of impurities.
Example Of Use
Austenitic steel for osteosynthetic prostheses biocompatible with the aggressiveness of all humours present in the human body with a metal structure designed to avoid all forms of metallosis, in the case of implants for reducing fractures.
Quality
The quality of EUREINOX products is closely linked to the quality of raw materials used. To this end, we have been able to establish valuable relationships with the best European steel mills over the years, thereby allowing us to utilize the highest quality materials available on the market in our production lines and optimize on our experience in casting.
The complete list of products is also in Eure Inox catalogue.
EURE+ Materials
The materials indicated with “+” can also be provided in the Eure+ type. They are materials obtained through a process of fabrication that makes them suitable for high speeds and for the use on automatic machines.