AISI: –
EN: 1,4106
C max: 0,03
Mn max: 2,00
P max: 0,040
S max: 0,25÷0,35
Si max: 2,00
Cr: 17÷19
Ni: –
Mo: 1,5÷2,5
Altri: –

Chemical Analysis
Characteristics
Ferromagnetic stainless steel with magnetic hysteresis at a low residual magnetization, optimizes low values of coercive force of Hc 140-160 A/Mt, equivalent to 1.82-2,00 Os without any deterioration in the resistance to intercrystalline corrosion and pitting on this object.
Example Of Use
Comparable to the austenitic stainless steel in consideration of its excellent self-lubrication, it is used in the production of cores for solenoids for which an high productivity on automatic lathes is required. It is also used in the production of solenoid valves and in the car industry.
Quality
The quality of EUREINOX products is closely linked to the quality of raw materials used. To this end, we have been able to establish valuable relationships with the best European steel mills over the years, thereby allowing us to utilize the highest quality materials available on the market in our production lines and optimize on our experience in casting.
The complete list of products is also in Eure Inox catalogue.
EURE+ Materials
The materials indicated with “+” can also be provided in the Eure+ type. They are materials obtained through a process of fabrication that makes them suitable for high speeds and for the use on automatic machines.